A 1" diamond core drill bit is $77 from Mcmaster-Carr but you will  
need to buy or more likely rent the drill rig to operate it as they  
have a threaded shank that does not fit the standard portable drills.  
They need to run at different speed and with coolant or you will burn  
the diamonds off the end of the bit.