Hey Dave; Using tie wire for gas rod seems to be slightly better
than store bought....thanks!...pete
Dave Smucker wrote:
> You should be able to find "tie wire" in both 16 and 10 gauge (or close
> to these sizes). This tie wire is used for tying rebar etc. Also called
> bailing wire, as older bailers used a similar wire to tie hay bails. I
> believe most of this wire is made from 1006 or 1008, very low carbon,
> low alloy steel.
>
> Dave
>
>> From: Peter Fels And Phoebe Palmer <artgawk at thegrid.net>
>> Reply-To: artgawk at thegrid.net,Sponsored by ABANA
>> <theforge at mailman.qth.net>
>> To: Sponsored by ABANA <theforge at mailman.qth.net>
>> Subject: [TheForge] pure iron wire?
>> Date: Mon, 12 Mar 2007 22:35:15 -0800
>>
>> Been frustrated trying to forge torch welded parts and sheet.
>> The available rods have alloying elements designed to work as
>> deposited...not forged, reheated, rewelded, hammered cold and hot and
>> so on.
>> So i thought...would pure iron welding rod work?
>> If so, where can i get some?
>> AK steel no longer lists it apparently....pete f
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> password: anvil
>>> ___________
>>>
>>>
>>>
>>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
More information about the TheForge
mailing list