I do have a propane weed burner, but I don't think that would get the horn up to forging temp. would it?
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Ron Childers
Sent: Wed 5/24/2006 11:40 AM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] ranite hardfacing rods
A propane weed burner should do it.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Darrell
Sent: Wednesday, May 24, 2006 12:32 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] ranite hardfacing rods
You just have to keep the face cool. The rest doesn't matter.
You should be able to rent a rosebud. Keep the heat out on the point.
Darrell
----- Original Message -----
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, May 24, 2006 7:21 AM
Subject: RE: [TheForge] ranite hardfacing rods
Peter, I may try that if I can borrow a large rosebud from someone. What do
you think about submerging all but the horn in a tub of water so as not to
disturb the face?