You may have to can it with a refractory to concentrate the heat but it
should do it 

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Washington, Aubrey O.
Sent: Wednesday, May 24, 2006 2:59 PM
To: Sponsored by ABANA
Subject: RE: [TheForge] ranite hardfacing rods

I do have a propane weed burner, but I don't think that would get the horn
up to forging temp. would it?

________________________________

From: theforge-bounces at mailman.qth.net on behalf of Ron Childers
Sent: Wed 5/24/2006 11:40 AM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] ranite hardfacing rods



A propane weed burner should do it.

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Darrell
Sent: Wednesday, May 24, 2006 12:32 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] ranite hardfacing rods

You just have to keep the face cool. The rest doesn't matter.
You should be able to rent a rosebud. Keep the heat out on the point.

Darrell

----- Original Message -----
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, May 24, 2006 7:21 AM
Subject: RE: [TheForge] ranite hardfacing rods


Peter, I may try that if I can borrow a large rosebud from someone.  What do

you think about submerging all but the horn in a tub of water so as not to
disturb the face?