[TheForge] ranite hardfacing rods

Ron Childers munlaw2 at hcsmail.com
Wed May 24 12:40:42 EDT 2006


A propane weed burner should do it.

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Darrell
Sent: Wednesday, May 24, 2006 12:32 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] ranite hardfacing rods

You just have to keep the face cool. The rest doesn't matter.
You should be able to rent a rosebud. Keep the heat out on the point.

Darrell

----- Original Message ----- 
From: "Washington, Aubrey O." <awashington at ou.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, May 24, 2006 7:21 AM
Subject: RE: [TheForge] ranite hardfacing rods


Peter, I may try that if I can borrow a large rosebud from someone.  What do

you think about submerging all but the horn in a tub of water so as not to 
disturb the face?

________________________________

From: theforge-bounces at mailman.qth.net on behalf of Peter Fels And Phoebe 
Palmer
Sent: Tue 5/23/2006 9:49 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] ranite hardfacing rods



You should be able to reforge it just fine Aubrey...PF






----------------------------------------------------------------------------
----


> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list