Washington, Aubrey O. wrote:
> Mouse Hole... tip of the horn is mushroomed...
> any of you ever tried reforging the wrought iron tip of a horn?
Rosebud. Heat tip to bright yellow. reforge using a hammer and either
another hammer as a dolly, or a real dolly. Be sure to secure the anvil
so it doesn't walk around as you attempt to reforge the horn. You can
even tack it to a welding table. Just make sure it is fast.
You can also place a wet towel on the face to sink away heat from the body.
> What are the hazards?
Hands in close proximity to that much heat always demands strong
caution and awareness. Two people are probably better for this job than
one.