[TheForge] Re: Pure Iron
Ries Niemi
rniemi at fidalgo.net
Sun Jun 11 18:40:16 EDT 2006
J.G. Braun, one of the Wagner companies, is going to start importing
Pure Iron again this summer, so it will be regularly available.
Not sure if it is up on their website yet, but it should be soon.
> http://www.jgbraun.com/pages/Jgbraun.html
Ries
On Jun 11, 2006, at 2:35 PM, LrdThorolf at aol.com wrote:
> put a chunk of cold pure iron through the power hammer and acts like
> it is
> clay or plastic. Got to watch guys playing with 3/4 inch pure iron
> through a
> Kuhn 150# while it was cold at ABANA 2000 conference in Flagstaff.
> I still got 1 small piece about 18" by 3' left.
> Does anyone know if there is anyone out there selling it or has some
> they
> want to sell in the midwest area. I.E. Michigan area?
> Yea I finally got forge set up after 3 years of being in storage. Can
> play
> now.
>
> Later Ike
> Pan's Forge.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
Ries Niemi
Industrial Artist
http://www.RiesNiemi.com
More information about the TheForge