[TheForge] Re: Pure Iron
Ries Niemi
rniemi at fidalgo.net
Sun Jun 11 18:48:10 EDT 2006
On Jun 11, 2006, at 3:40 PM, Ries Niemi wrote:
> J.G. Braun, one of the Wagner companies, is going to start importing
> Pure Iron again this summer, so it will be regularly available.
> Not sure if it is up on their website yet, but it should be soon.
>> http://www.jgbraun.com/
Try this link- the first one doesnt work.
> Ries
>
>
> On Jun 11, 2006, at 2:35 PM, LrdThorolf at aol.com wrote:
>
>> put a chunk of cold pure iron through the power hammer and acts like
>> it is
>> clay or plastic. Got to watch guys playing with 3/4 inch pure iron
>> through a
>> Kuhn 150# while it was cold at ABANA 2000 conference in Flagstaff.
>> I still got 1 small piece about 18" by 3' left.
>> Does anyone know if there is anyone out there selling it or has some
>> they
>> want to sell in the midwest area. I.E. Michigan area?
>> Yea I finally got forge set up after 3 years of being in storage. Can
>> play
>> now.
>>
>> Later Ike
>> Pan's Forge.
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
> Ries Niemi
> Industrial Artist
>
> http://www.RiesNiemi.com
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
Ries Niemi
Industrial Artist
http://www.RiesNiemi.com
More information about the TheForge