put a chunk of cold pure iron through the power hammer and acts like it is  
clay or plastic. Got to watch guys playing with 3/4 inch pure iron through a  
Kuhn  150# while it was cold at ABANA 2000  conference in Flagstaff. 
I still got 1 small piece about 18" by 3' left.