FWIW,
different glass manufacturers have slightly different specs. But in
the same ballpark. :)
For Bullseye Glass....
slumping...................with no thickness change.... is done
between 1200 F and 1290 F.
bill
On Jun 11, 2006, at 2:42 PM, Bob Ehrenberger wrote:
> Ralph,
>
> We have a shop near here that specilizes in slumped and fused glass
> art.
>
> She showed me her kiln and said that she runs it at 500F. Takes
> several
> hours at that temp, It would be faster at a higher temp but you
> would loose
> some control.
>
> Robert Ehrenberger