Sure.
Pull the wire out of your mig gun and grind a tungsten
tig tip to fit in the mig's contact tip. You now have a
scratch start tig gun.
Use argon.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Fiorini & Skiles" <bkmetal at mwt.net>
>
> I know that tig welding is ideal for bronze, but we
> don't have one. Has anyone set up a mig for welding
> bronze? The sculptor at UW-L does this for touching
> up bronze castings.
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list