[TheForge] Welding Rod

Ron Childers munlaw2 at hcsmail.com
Thu Jun 8 09:40:29 EDT 2006


E6011= 60k psi ts AC or DC + or - all position, general purpose - Works on
dirty or rusted metal. E7014= 70K psi ts AC or DC + or- all position- used
for lap & fillet welds- likes a clean surface. Google Lincoln consumables.
You can get a brochure listing the rods and general information about each.

Ron Childers

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Rick
Sent: Thursday, June 08, 2006 7:52 AM
To: theforge at mailman.qth.net
Subject: [TheForge] Welding Rod

Hi folks -

    I am in the midst of a dilemma.  I used to weld every day, and got 
pretty good at it, but never learned about picking out which rod to use.  (I

was primarily a layout man and only welded to fill in.)  I have heard 7018 
touted as a good all around rod.  I had some 7014 rod here that was probably

10-12 years old and never in a rod cabinet, since I don't have one.  It also

gets quite humid here in the summer.  That 7014 rod worked great the other 
day when I used it.  The 6011 or 6013 I had wouldn't work near as well.

    Can someone tell me what the letters mean?  I know the first tells 
tensile strength, but what do the others mean?


Thanks,

Rick Crawford at Rafter Lazy C
  Home of Smoky Forge and Lem the Wonder Mule
   In the middle of Northern Illinois

    http://www.smokyforge.com
     rick at smokyforge.com 



-- 
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.394 / Virus Database: 268.8.1/355 - Release Date: 6/2/2006

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list