[TheForge] Welding Rod
Rick
rick at smokyforge.com
Thu Jun 8 07:51:58 EDT 2006
Hi folks -
I am in the midst of a dilemma. I used to weld every day, and got
pretty good at it, but never learned about picking out which rod to use. (I
was primarily a layout man and only welded to fill in.) I have heard 7018
touted as a good all around rod. I had some 7014 rod here that was probably
10-12 years old and never in a rod cabinet, since I don't have one. It also
gets quite humid here in the summer. That 7014 rod worked great the other
day when I used it. The 6011 or 6013 I had wouldn't work near as well.
Can someone tell me what the letters mean? I know the first tells
tensile strength, but what do the others mean?
Thanks,
Rick Crawford at Rafter Lazy C
Home of Smoky Forge and Lem the Wonder Mule
In the middle of Northern Illinois
http://www.smokyforge.com
rick at smokyforge.com
--
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.394 / Virus Database: 268.8.1/355 - Release Date: 6/2/2006
More information about the TheForge
mailing list