[TheForge] Welding Rod
Ron Childers
munlaw2 at hcsmail.com
Thu Jun 8 10:26:26 EDT 2006
Rick,
Check the end of the rod that goes in the electrode holder and clean off the
rust- 6010 (5P) or 6011 should work when wet- you may have to run a bit
hotter... 6010 is for DC reverse polarity. They will work on AC if run at
more heat than used with 6011.
Ron Childers
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Ron Childers
Sent: Thursday, June 08, 2006 9:40 AM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] Welding Rod
E6011= 60k psi ts AC or DC + or - all position, general purpose - Works on
dirty or rusted metal. E7014= 70K psi ts AC or DC + or- all position- used
for lap & fillet welds- likes a clean surface. Google Lincoln consumables.
You can get a brochure listing the rods and general information about each.
Ron Childers
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Rick
Sent: Thursday, June 08, 2006 7:52 AM
To: theforge at mailman.qth.net
Subject: [TheForge] Welding Rod
Hi folks -
I am in the midst of a dilemma. I used to weld every day, and got
pretty good at it, but never learned about picking out which rod to use. (I
was primarily a layout man and only welded to fill in.) I have heard 7018
touted as a good all around rod. I had some 7014 rod here that was probably
10-12 years old and never in a rod cabinet, since I don't have one. It also
gets quite humid here in the summer. That 7014 rod worked great the other
day when I used it. The 6011 or 6013 I had wouldn't work near as well.
Can someone tell me what the letters mean? I know the first tells
tensile strength, but what do the others mean?
Thanks,
Rick Crawford at Rafter Lazy C
Home of Smoky Forge and Lem the Wonder Mule
In the middle of Northern Illinois
http://www.smokyforge.com
rick at smokyforge.com
--
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.394 / Virus Database: 268.8.1/355 - Release Date: 6/2/2006
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list