[TheForge] Forge Lining
Rick
rick at smokyforge.com
Sat Jul 22 08:13:56 EDT 2006
That sounds nice, Jay, but what is your web site address? I might like to
look at what you have to offer.
Rick Crawford at Rafter Lazy C
Home of Smoky Forge and Lem the Wonder Mule
In the middle of Northern Illinois
http://www.smokyforge.com
rick at smokyforge.com
----- Original Message -----
From: "Jay Hayes" <xmas4lites at earthlink.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, July 21, 2006 8:32 PM
Subject: Re: [TheForge] Forge Lining
> Hey Mikey,
>
> I thought I sent you some information about the Clamshell and Super Wide
> Oval Forges a while back. We have been making them for several years. I'll
> have to send you some pictures.
>
> We make both types in three standard sizes as well as custom sizes. The
> standard kits are: a Single Burner 16W x 12H x 12L, a Two Burner 16W x
> 12H x 18L, and a Three Burner 16W x 12H x 24L Both the Clamshell and
> Oval formats are more practical and efficient than a similar sized
> cylindrical forge.
>
> The Clamshell Forges have a full width flat floor that is insulated with
> three inches of Ceramic Fiber and Super Duty Floor Bricks. The upper
> section of the Clamshell Forge, also insulated with three inches of
> ceramic fiber, can either hinge from one side or completely lift off the
> floor section.
>
> This versatility allows huge parts to have sections heated that would not
> normally be able to fit into other gas forges. It is great for things like
> large scrolls, assembled sections, and armor. When the Clamshell is
> closed, work can be loaded from the front or rear of the forge. Long parts
> can run completely through the forge. Our CNC plasma cut end plates have a
> small port in the door to allow necessary exhaust gases to escape while
> maintaining maximum heat retention. The doors can be configured a number
> of ways to suit the builder and the type of work.
>
> All of the forge kits feature our 3/4 inch high output, High Performance
> Burners and a Fuel Saver Valve Manifold. These burners are equipped with a
> specifically designed gas orifice, a machined nozzle, and integral choke
> plate. A wide range of adjustment allows the burners to be easily tuned to
> run stable from less than one psi to well over 25 psi. Each burner of our
> multi burner forge kits has its own shutoff valve, so gas is supplied only
> to the burners needed for the job. The valve manifold also has a low
> pressure Fuel Saver idle circuit that cuts all the burners back to a low
> fire when the work is moved to the anvil.
> The net result is a very versatile industrial quality forge that heats up
> fast, is easy to use, and gets the maximum use out of a tank of gas.
>
> Jay
--
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.394 / Virus Database: 268.10.3/395 - Release Date: 7/21/2006
More information about the TheForge
mailing list