Hey Mikey,

I thought I sent you some information about the Clamshell and Super Wide 
Oval Forges a while back. We have been making them for several years. 
I'll have to send you some pictures.

We make both types in three standard sizes as well as custom sizes. The 
standard kits are: a Single Burner 16W x 12H x 12L,  a Two Burner 16W x 
12H x 18L,  and a Three Burner 16W x 12H x 24L  Both the Clamshell and 
Oval formats are more practical and efficient than a similar sized 
cylindrical forge.

The Clamshell Forges have a full width flat floor that is insulated with 
three inches of Ceramic Fiber and  Super Duty Floor Bricks. The upper 
section of the Clamshell Forge, also insulated with three inches of 
ceramic fiber, can either hinge from one side or completely lift off the 
floor section.

This versatility allows huge parts to have sections heated that would 
not normally be able to fit into other gas forges. It is great for 
things like large scrolls, assembled sections, and armor. When the 
Clamshell is closed, work can be loaded from the front or rear of the 
forge. Long parts can run completely through the forge. Our CNC plasma 
cut end plates have a small port in the door to allow necessary exhaust 
gases to escape while maintaining maximum heat retention. The doors can 
be configured a number of ways to suit the builder and the type of work.

All of the forge kits feature our 3/4 inch high output, High Performance 
Burners and a Fuel Saver Valve Manifold. These burners are equipped with 
a specifically designed gas orifice, a machined nozzle, and integral 
choke plate. A wide range of adjustment allows the burners to be easily 
tuned to run stable from less than one psi to well over 25 psi. Each 
burner of our multi burner forge kits has its own shutoff valve, so gas 
is supplied only to the burners needed for the job. The valve manifold 
also has a low pressure Fuel Saver idle circuit that cuts all the 
burners back to a low fire when the work is moved to the anvil.
The net result is a very versatile industrial quality forge that heats 
up fast, is easy to use, and gets the maximum use out of a tank of gas.

Jay


Mike Porter wrote:

>Hi Jay,
>This is the first I've heard about your clamshell forges. You need to write
>more on the group.
>Mikey
>
>-----Original Message-----
>From: theforge-bounces at mailman.qth.net
>[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jay Hayes
>Sent: Thursday, July 20, 2006 3:56 PM
>To: Sponsored by ABANA
>Subject: Re: [TheForge] Forge Lining
>
>Luke,
>
>I also carry regulators and everything else needed to build gas forges. 
>I also have a number of forge kits including several clamshell forge kits.
>
>As others mentioned check the temperature ratings of the ceramic fiber 
>and other refractory. You can use lower temp material behind higher temp 
>refractory, but low temp stuff will not hold by itself up to the high 
>heat of a forge. I prefer three inches of ceramic fiber for better fuel 
>economy, although a lot of folks only use two inches.
>
>Jay Hayes
>jay at hrea.coop
>
>
>Luke Thomson wrote:
>
>  
>
>>My friend's uncle is a refractory man, i don't know exactly what his
>>position is but he's some sort of contractor for refractory and fire
>>insulating work. That's insignificant though, the cool part is I get free
>>refractories!!!
>>
>>Here's What I Got:
>>1. 1" thick Kao-wool, durablanket or some brand of refractory blanket
>>2. ***Naphos-85   i have a couple gallons and with it Matt (refractory
>>hook-up) said "holds brick together up to .25"  thick" and "add water 
>>to get
>>consistency of morter/slurry"
>>3. ***Ply Brico "trawelable* plastic .5" to 3" thick" and "fills cracks &
>>voids etc. where there isn't a brick" *Real Sticky*
>>4. bag of AP Green Castable refractory
>>                        ***He also said that both the 'ply brico' and
>>'naphos' are 85% alumina where the standard is 50%
>>
>>Here is what I want:
>>A forge... I cut the ends of a propane tank and burned the paint off 
>>for a
>>forge shell. I'm not neccessarily set on this but it seems like the right
>>size for my second forge, ( just today another friends dad gave me 
>>their old
>>forge to use while I build my own). The hope is that with those 
>>refractories
>>and one of mike porter's burners I'll have a forge pretty soon. I've 
>>already
>>forked out the big bucks and bought most of the parts for the .5 & .75"
>>burner's in his book.
>>
>>now for the actual questions:
>>1. I've read about Jerry using a couple layers of Kaowool protected by
>>refractory cement and rather liked the idea, but would like to hear
>>other suggestions considering the materials I have.
>>
>>2. If I decide to go with the two layers of kao-wool how thick should 
>>I lay
>>on the refrectory cement and which one should I use? should i do like 
>>.75"
>>on the top and sides and 1.5 or so inches on the bottom?
>>
>>3. Is there a website or anywhere in particular where I should buy a
>>regulator, or will most places pretty much be the same: central welding
>>supply, hardware store, etc.
>>
>>Any other suggestions?
>>
>>Thanks always for your advice,
>>Luke
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  blacksmithblacksmith at hotmail.com
>>password:  anvil
>>___________
>>
>>
>>
>>    
>>
>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  blacksmithblacksmith at hotmail.com
>password:  anvil
>___________
>
>
>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  blacksmithblacksmith at hotmail.com
>password:  anvil
>___________
>
>
>
>  
>




More information about the TheForge mailing list