[TheForge] slitting and drifting help needed

Washington, Aubrey O. awashington at ou.edu
Tue Feb 14 16:34:53 EST 2006


Dan, I think you and Bob are saying the same thing when Bob says the circ. "measured along both sides of the slit added together."

________________________________

From: theforge-bounces at mailman.qth.net on behalf of Dan Tull
Sent: Tue 2/14/2006 3:24 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] slitting and drifting help needed



How about half the circ.?
----- Original Message -----
From: "Bob Willman" <blcksmth at wcnet.org>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Tuesday, February 14, 2006 3:47 PM
Subject: RE: [TheForge] slitting and drifting help needed


> I would start with a slit that was almost equal to the circumference
> of the finished hole measured along both sides of the slit added together.
> This should drift out to very close to the diameter hole you need.
>
>
> Bob Willman
> Bowling Green, Ohio
> The Eagle's Anvil
> WB8NQW
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of robert hensarling
> Sent: Monday, February 13, 2006 8:38 PM
> To: theforge
> Subject: [TheForge] slitting and drifting help needed
>
> Guys, is there a reference, or chart maybe, of what size slitting chisel
> to
> use for a given drifted hole diameter?  In other words, if I want a
> drifted
> finished hole size to be 1/2", what size of slitting chisel would I use,
> not
> only for this size, but 3/16th's, 1/4, 3/8th's etc. I'm referring to the
> "canoe" shaped slitting chisel.
> I understand that a slit and drifted hole will increase the overall length
> of a given piece of steel, and a punched and drifted hole will in fact be
> a
> little less.  Do I have this correct, or am I backwards?
> Thanks for the info!
> Robert Hensarling
> Uvalde, Texas
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list