Paddy
Your anvil should have some "ring" Wilkinson's are wrought iron with
a welded steel face just like your Peter Wright. The only anvils that have
no ring are cast iron like Fishers.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of TOOL GYPSY
Sent: Saturday, April 22, 2006 10:49 AM
To: theforge at mailman.qth.net; The_Anvil at yahoogroups.com
Subject: [TheForge] To ring or not to ring[was anvil i d]
Wise sages
My anvil turned out to be a wilkinson.It easily has as much rebound
as my pw but the ring seems to be gone south.There are no thunks or burps
just an eerie quiet.I can see this as a qood thing as long as this is just a
quirk and not a structural problem.I have been told that some anvils do not
have a ring but are still excellent tools.Any one have a wilkinson minus the
rinq?All input would be apprietiated as i was planning on making this my new
no 1
Paddy p the wannabe
East of Cape Sable and west of Cape Canso
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list