[TheForge] Kaowool and Durablanket: apples and oranges
Mike Porter
michael.a.porter at comcast.net
Sun Apr 16 21:40:43 EDT 2006
Andy,
Not having used Durablanket I am not disputing your statement. However, I
mean to investigate it and hope to prove you quite... RIGHT. There is
nothing I like better than learning a better way to do things. However, this
is the first such comparison statement I have ever heard.
Mikey
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Steve Smith
Sent: Sunday, April 16, 2006 10:28 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Kaowool and Durablanket: apples and oranges
I've always used Durablanket and liked it (but this means I can't
compare). I was going to get Kaowool, but it turned out the sales guy
was reading me the destruct temp as a use temp. I went with the other
supplier which happened to have Durablanket.
Steve
Gladish Family wrote:
> Maybe it has been said, but from my experience, Durablanket and Kaowool
> are quite different products with different uses.
> As an insulating material, Kaowool is excellent, but it shouldn't be the
> final layer on the hot part of the forge.
> Durablanket performs the same task, with one huge difference: it
> reflects heat WAY better than Kaowool, meaning that your forge gets much
> hotter.
> Durablanket with a thin coating of Plistix- which Larry Zoeller sells-
> makes my dirt simple blown forge an outstanding welding machine. It gets
> seriously bright white hot in there, something I was not able to achieve
> with the same forge and Kaowool.
>
> Andy Gladish
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list