[TheForge] Kaowool and Durablanket: apples and oranges

Demon Buddha osan at netlabs.net
Tue Apr 18 09:02:42 EDT 2006



Jerry Frost wrote:
> Exactly.
> 
> I have an inner liner of 4,000f high phosphate rammable refractory about 
> 3/4" thick, surrounded with 1" 9oz Kaowool.
> 
> I should've used 2" of Kaowool. Next time.

	Graphite.