> ======= On 2005-09-28, at 07:29:18 Justin Fellenz wrote: =======
>
> >Rob or James or anyone else,
> >
> >Do you know if copper water pipe has beryllim in it?
>
> It doesn't. AFAIK, only big buss bars and some bushings should be
> approached with caution. :)
>
>