======= On 2005-09-28, at 07:29:18 Justin Fellenz wrote: ======= >Rob or James or anyone else, > >Do you know if copper water pipe has beryllim in it? It doesn't. AFAIK, only big buss bars and some bushings should be approached with caution. :) "Caesar si viveret, ad remum dareris." - Xanthippos Roy Wilson - rwilson9 at twcny.rr.com 2005-09-28