[TheForge] Anvil shaving 101
Ron Childers
munlaw2 at hcsmail.com
Thu May 26 14:22:12 EDT 2005
Paddy, don't do it- unless the face looks like furrows in a plowed field.
The hard face on most PW's look about 3/8". A sway will actually help in
straightening operations and most forging is done across the anvil any way,
and most smiths use the same 3 or 4 inches. Move your spot up toward the
horn, use it as-is and don't worry about it. Adds character. Besides 3/16"
is not that bad for an anvil with that long a striking surface.
Ron C
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of TOOL GYPSY
Sent: Thursday, May 26, 2005 2:01 PM
To: theforge at mailman.qth.net
Subject: [TheForge] Anvil shaving 101
Hello All
I have a 400 lb pw anvil that has a lot of sway.I was thinking about
having the top planed down by about 3/16 .Does anyone have an idea as to how
thick the hardened surface would be on an avvil this large?
Paddy P the wannabe
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list