>       I have a 400 lb pw anvil that has a lot of sway.I was thinking about
> having the top planed down by about 3/16 .Does anyone have an idea as to how
> thick the hardened surface would be on an avvil this large?
>                                           Paddy P the wannabe
Depends on who did what to it over the years.
Personally I would leave it alone. The sway is very helpfull for
straighting work.