It's been thirty years since HS shop, but I don't think that there was 
any more to the process than the weld...no post anneal.
The setup was exactly like what Mike describes at the Michelin wire 
mill. Pretty slick.

Ralph Sproul wrote:

>Andy,  I thought there was some annealing to be done in this process besides
>just butt weld and grind.  Maybe that's my problem.
>  
>

Andy Gladish, Metalwork
7141 Guemes Island Rd.
Anacortes, WA 98221
Element Forge  www.elementfe.com
mailto: andy at elementfe.com

I never saw an ugly thing in my life: for let the form of an object be what
it may, -- light, shade, and perspective will always make it beautiful.