I sell two different materials that are a great replacement for ITC 100 at
a substantial savings, I have the Plistix 900F and QF-180 and they both
have the high thermal reflective properties that you need.  And if you feel
like driving to Kentucky you can pick it up also.
The following URL will have more information.
http://www.geocities.com/zoellerforge/flare.html
I try not to push my products an the list, but with this thread I feel it
is valuable information that could be added.
Thanks,
Larry Zoeller
4312 Lahnna Dr.
Louisville, KY 40216
zman59 at earthlink.net
www.geocities.com/zoellerforge


> [Original Message]
> From: S. Pohlman <ajarrod at voyager.net>
> To: Schade <schade at acegroup.cc>; the forge <theforge at mailman.qth.net>
> Date: 3/30/2005 6:21:57 PM
> Subject: Re: [TheForge] local source of ITC 100
>
>  Centaur forge is great for alot of things however they do not carry any 
> ITC 100 or other refractory material. just rebuild kits for the forges 
> they sell. when I called  they hadn't even herd of it.
>    someone mentioned plistix how does that compare? or the fibrefrax 180 
> blue
>
> Schade wrote:
>
> > Stu,
> >
> > You can't be much more than a hour from Centaur if you wanna buy in 
> > person. My map shows about 40 miles (Lake Zurich, IL to Burlington, 
> > WI). I would consider that pretty local for a somewhat specialized item.
> >
> > Another online source would be Larry Zoeller also on this list.
> >
> > Bob
> > ______
> >
> >
> > On Mar 29, 2005, at 5:09 PM, S. Pohlman wrote:
> >
> >> I live in the North East corner of Illinois.  Lake Zurich in Lake 
> >> county to be exact. Centaur forge is great for most stuff but I am re 
> >> doing my gas forge and want to find a local source for  itc100 
> >> refractory. any help would be a great . I have seen it for sale on 
> >> the net but prefer to buy in person.
> >>
> >> Stu
> >>
> >>
> >
> >
> >
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>




More information about the TheForge mailing list