[TheForge] local source of ITC 100

S. Pohlman ajarrod at voyager.net
Wed Mar 30 19:23:58 EST 2005


 Centaur forge is great for alot of things however they do not carry any 
ITC 100 or other refractory material. just rebuild kits for the forges 
they sell. when I called  they hadn't even herd of it.
   someone mentioned plistix how does that compare? or the fibrefrax 180 
blue

Schade wrote:

> Stu,
>
> You can't be much more than a hour from Centaur if you wanna buy in 
> person. My map shows about 40 miles (Lake Zurich, IL to Burlington, 
> WI). I would consider that pretty local for a somewhat specialized item.
>
> Another online source would be Larry Zoeller also on this list.
>
> Bob
> ______
>
>
> On Mar 29, 2005, at 5:09 PM, S. Pohlman wrote:
>
>> I live in the North East corner of Illinois.  Lake Zurich in Lake 
>> county to be exact. Centaur forge is great for most stuff but I am re 
>> doing my gas forge and want to find a local source for  itc100 
>> refractory. any help would be a great . I have seen it for sale on 
>> the net but prefer to buy in person.
>>
>> Stu
>>
>>
>
>
>