>What do you have under the anvil?Is it build on heavy plate? 30" of 5" 
>shaft is only about 165 lbs. by my figures. 25 pound Little giant is about 
>800lbs. with most of the weight in the anvil and it has a rigid frame.I 
>used a 6" shaft for my anvil but mounted it on top of a 4" thick plate 
>that weighs 1500LBs. and it works fine.I think your hammer to anvil weight 
>ratio is causing allot of your problems.
>
>
>---
>Mark & Sylvia Mondloch
>Silver Creek Pottery & Forge
>W6725 Hwy 144
>Random Lake ,Wi 53075
>HotArt at silvercreekpottery.com
>http://www.silvercreekpottery.com
>----- Original Message ----- From: "kim george" <klgeorge at kent.edu>
>To: <knife-list at kepler-eng.com>; <theforge at mailman.qth.net>
>Sent: Wednesday, March 23, 2005 4:41 PM
>Subject: [TheForge] air hammer-2
>
>
>>First the hammer is modified Kenyon that I cobbled together :-)).  The 
>>hammer is approximately 60# the anvil is 30" of 5" shafting. The whole 
>>thing weighs about 800#. The reason I don't want to cut the floor is that 
>>it was built over an old chicken coop floor and foundation, back filled 
>>with field stone.
>>         The problem is that the back foundation is sinking and that is 
>> 15' from the hammer. I'm trying to slow the process down so that in 30 
>> years when I quit I haven't had to rebuild the shop 3or4 times. We have 
>> definite water problems, a spring 10' off the back corner.
>>         Now if I win the lottery the subject will be moot. Because I'll 
>> be building a bigger shop on a different piece of ground with room for 
>> more toys.;-))
>>
>>
>>Kim George
>>
>>       "Why for you burry me in cold,cold ground?" Taz
>>
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  blacksmithblacksmith at hotmail.com
>>password:  anvil
>>___________
>>
>>
>
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  blacksmithblacksmith at hotmail.com
>password:  anvil
>___________
>
>




More information about the TheForge mailing list