[TheForge] Putting an oxide finish on mild steel?

xlch58 at swbell.net xlch58 at swbell.net
Sun Mar 13 11:20:39 EST 2005


It would also obscure the oxides over time as well.

Charles

Andrew Vida wrote:

>     Linseed oil polymerizes with time and heat.  I can't recommend it 
> for outside use, but it's great inside if it's not being abused too much.