Barking Crow wrote:
> This afternoon after returning from a FABA meeting (smithing content) I was
> welding a thumb screw type tab on a bolt that didn't have much length so i
> wanted to protect the threads from the molten rod/splatter and put a length
> of scrap copper tubing over the threads knowing as I do that the 6013
> wouldn't weld to the copper since I sometimes use a copper damn to stop the
> molten rod. But, you guessed it, the weld attachen the copper tubing rather
> well to the bolt and I got to chisel, pry and grind the copper from the
> bolt. Does this surprise those of you who know which is the shinola.
If all you were looking to do was keep splatter off, you might try
sooting the threads up real nice with acetylene. Threads should stay
clean as long as the weld puddle doesn't actually wander too close.