> This afternoon after returning from a FABA meeting (smithing content) I
was
> welding a thumb screw type tab on a bolt that didn't have much length so i
> wanted to protect the threads from the molten rod/splatter and put a
length
> of scrap copper tubing over the threads knowing as I do that the 6013
> wouldn't weld to the copper since I sometimes use a copper damn to stop
the
> molten rod.  But, you guessed it, the weld attachen the copper tubing
rather
> well to the bolt and I got to chisel, pry and grind the copper from the
> bolt.  Does this surprise those of you who know which is the shinola.
>
> Jeff in already 75 degrees Tallahassee
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>



More information about the TheForge mailing list