[TheForge] RE: Smithing Question - Hold down
Steve Smith
sos at alum.mit.edu
Tue Mar 8 22:08:38 EST 2005
I use a timing chain out of a Porsche 911 attached to a weight. It works
very nicely.
Steve
Bob Ehrenberger wrote:
> When I need a hold down I use my saddle anvil in the hardy hole. Just lift
> it up slide the work under and give it a tap to tighten it up. It only
> takes about two seconds and the work is still hot.
>
> I'm not sure I have the term right, but what I call a saddle anvil is a
> piece of leaf spring that has been bent into an "n" shape and welded to a
> post for the hardy hole.
>
>
> Steve Austin had spring loaded hold down that is foot opperated. It is fast
> and easy to use but looked like it was in the way all the time when not in
> use. It might have had an easy way to move it out of the way but he left it
> in place the day I was there.
>
> Pat McCarty has a hold down made from a pipe clamp. It just screwed down to
> hold the work.
>
> You can always just use a loop of chain with a heavy weight on it.
>
> Robert Ehrenberger
> Shelbyville, Mo.
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list