[TheForge] Black finish for galvanized

Kevin Donahoe flyinpig at go-concepts.com
Fri Mar 4 08:12:07 EST 2005


Rick,

That website is Beach Island Group... is that who you're doing the work for
or supposed to be the galvanizer?

Really nice spread in the AR, congratulations.  I forget, do you have a
website featuring your work?

Kevin

 -----Original Message-----
 From: theforge-bounces at mailman.qth.net
 [mailto:theforge-bounces at mailman.qth.net]On Behalf Of RICK KORINEK
 Sent: Thursday, March 03, 2005 9:33 PM
 To: Sponsored by ABANA
 Subject: Re: [TheForge] Black finish for galvanized


 Andy, its not too late but there's not enough budget to begin
 to consider stainless.  Also, I found a large and reputable
 plater out here, Duncan Group, who have a stain after galv.
 I talked with them today.  It is only recommended in parking
 garages and other non-critical areas as it is not
 particularly attactive.  They have tried it on several
 residential projects and have had to bead blast it off to
 satisfy the customers.  It sounds like is is a thin stain and
 not a chemical that reacts with the zink.

 They do have several paint coatings that they have engineered
 for coating over galvanized, including acrylic, polyutethane
 and a hard and soft powder coat.  They apply and warranty.
 Some good info on their website: duncangroup.com, I think.

 -Rick




 ---- Original message ----
 >Date: Thu, 03 Mar 2005 10:16:12 -0500
 >From: Andrew Vida <osan at netlabs.net>
 >Subject: Re: [TheForge] Black finish for galvanized
 >To: Sponsored by ABANA <theforge at mailman.qth.net>
 >
 >
 >
 >RICK KORINEK wrote:
 >> I am working on an exterior railing that will be installed
 >> near the ocean.  I am looking seriously into having it hot-
 >> dipped.
 >
 >	A bit late in the game, I suppose, but didn't you
 consider using stainless?
 >_______________________________________________
 >Manage membership or unsubscribe at:
 >http://mailman.qth.net/mailman/listinfo/theforge
 >theforge mail list group photo site is
 >http://www.photoaccess.com
 >Login:  blacksmithblacksmith at hotmail.com
 >password:  anvil
 >___________
 >
 >
 Rick Korinek
 Emerald City Forge
 Framingham, MA
 _______________________________________________
 Manage membership or unsubscribe at:
 http://mailman.qth.net/mailman/listinfo/theforge
 theforge mail list group photo site is
 http://www.photoaccess.com
 Login:  blacksmithblacksmith at hotmail.com
 password:  anvil
 ___________







More information about the TheForge mailing list