[TheForge] Black finish for galvanized
RICK KORINEK
rickkorinek at rcn.com
Thu Mar 3 21:32:55 EST 2005
Andy, its not too late but there's not enough budget to begin
to consider stainless. Also, I found a large and reputable
plater out here, Duncan Group, who have a stain after galv.
I talked with them today. It is only recommended in parking
garages and other non-critical areas as it is not
particularly attactive. They have tried it on several
residential projects and have had to bead blast it off to
satisfy the customers. It sounds like is is a thin stain and
not a chemical that reacts with the zink.
They do have several paint coatings that they have engineered
for coating over galvanized, including acrylic, polyutethane
and a hard and soft powder coat. They apply and warranty.
Some good info on their website: duncangroup.com, I think.
-Rick
---- Original message ----
>Date: Thu, 03 Mar 2005 10:16:12 -0500
>From: Andrew Vida <osan at netlabs.net>
>Subject: Re: [TheForge] Black finish for galvanized
>To: Sponsored by ABANA <theforge at mailman.qth.net>
>
>
>
>RICK KORINEK wrote:
>> I am working on an exterior railing that will be installed
>> near the ocean. I am looking seriously into having it hot-
>> dipped.
>
> A bit late in the game, I suppose, but didn't you
consider using stainless?
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
Rick Korinek
Emerald City Forge
Framingham, MA
More information about the TheForge
mailing list