I calculated the weight difference between the 1.25"
and the 1.5" plate for 16" X 41", and it's only 47
pounds.  Is that enough of a difference in the base
plate to matter?

--- Dave Mudge <dave at magichammer.net> wrote:

> Figure out how much 1-1/4 plate x the length of the
> plate called for in the
> plans, and have your 1-1/4 inch plate made that much
> wider.
> 
> dave mudge
> dave at magichammer.net
> http://www.magichammer.net
> http://www.metalsmithinghowto.com
>  
> 
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf
> Of Phil
> Sent: Thursday, June 09, 2005 4:10 PM
> To: Sponsored by ABANA
> Subject: [TheForge] Air Hammer Base Plate
> 
> I'm builing the standard size Kinyon, from the ABANA
> plans.  The place I get my steel from doesn't have
> 1.5" plate for the base plate.  They do have 1.25"
> plate.  
> Would that be thick enough?
> 
> 
> 		
> __________________________________ 
> Discover Yahoo! 
> Use Yahoo! to plan a weekend, have fun online and
> more. Check it out! 
> http://discover.yahoo.com/
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 



		
__________________________________ 
Discover Yahoo! 
Find restaurants, movies, travel and more fun for the weekend. Check it out! 
http://discover.yahoo.com/weekend.html 



More information about the TheForge mailing list