Steve Hurlock wrote:
>
> Has anyone ever made a Log Dog? How long? What size stock? Do they need to be hardened?
> Thanks, Steve
> ___________
The ones I have seen were usually about 14 inches long and the arms (
part that goes in log) was about 3 inches long. Had a crosssection of
5/8th in ( I think)
Ralph
--