Clamping to a welding table will usually do the trick.  What in 
particular do you have in mind?

Fiorini & Skiles wrote:
> When creating a rectangular frame from strap steel, is there any way to
> prevent warping?  Is there any magic way to fix it, other than beating the
> heck out of it?
> -Kirsten