define the strap (ie: 1/4" x 1").
what are the dimensions of the frame?
is the whole piece warping (as in away from the table that you lay it
out on)
or is the piece of strap warping (as in left or right from it's own axis) ?
what type of corner joint/ fastener?
dm
Fiorini & Skiles wrote:
>When creating a rectangular frame from strap steel, is there any way to
>prevent warping? Is there any magic way to fix it, other than beating the
>heck out of it?
>-Kirsten
> bkmetal at mwt.net
>http://www.mwt.net/~bkmetal/index.html
>Japanese Forging Hammers at http://www.mwt.net/~bkmetal/Billhome.html
>
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
>
>
>
>
>
--
No virus found in this outgoing message.
Checked by AVG Anti-Virus.
Version: 7.0.300 / Virus Database: 265.8.8 - Release Date: 2/14/2005
More information about the TheForge
mailing list