Fred,
Ignorance can lead one (me) to be either too cautious or too bold.
Aubrey
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Fred Zickrick
Sent: Mon 12/12/2005 7:09 PM
To: theforge at mailman.qth.net
Subject: [TheForge] Re: TheForge Digest, Vol 23, Issue 22
At 01:08 PM 12/12/2005, you wrote:
>For those following the saga of the broke cast iron post drill
>part: Over the weekend I got started forging a replacement
>part. (Only had a couple of hours in the shop, so I didn't get it
>finished.) My plan is to try brazing the original after I get the
>replacement finished.
>
>Aubrey
Way too cautious! :-)
"Those who would give up essential Liberty, to purchase a little
temporary Safety, deserve neither Liberty nor Safety."
Benjamin
Franklin, 1755
Fred & Marilyn
fredz72 at cableone.net
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list