About 3 tons, can't you do the math? I use 0.3 pounds per cubic inch.(.28
is a little better) 14 feet equals 168 inches, 7 foot 7 equals 91 inches,
So the volume is equal to 168 x 91 x 1.25 = 19110 cubic inches. Take the
volume times 0.3 equals 5733 pounds or a little less than 3 tons.
Dave
----- Original Message -----
From: <SRiverF at aol.com>
To: <theforge at mailman.qth.net>
Sent: Monday, April 25, 2005 8:01 PM
Subject: [TheForge] table weight
>I have someone selling me a table for the scrap weight, Can anyone tell me
> what a table 14' X 7' - 7" x 1& 1/4" thick would weight?
>
> /Thanks
> Mike IVey
> Savannah River Forge
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list