diameter x diameter x length (inches) X 0.2229 equals weight per inch 
of round bar.
width x thickness x length (inches) x 0.2833 weight per inch of flats 
or squre stock.
Mike Schermerhorn

-----Original Message-----
From: Ron Childers <munlaw2 at hcsmail.com>
To: 'Sponsored by ABANA' <theforge at mailman.qth.net>
Sent: Mon, 18 Apr 2005 13:21:27 -0400
Subject: RE: [TheForge] Steel weight

Also Machinery's Handbook

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of gblacksmith
Sent: Saturday, April 16, 2005 6:05 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Steel weight

Folks:  There is a very nice chart available from Kirkpatrick Forge and
Welding in Willits, CA, for about 13.00.  It shows weights for all 
common
steel shapes, by the foot, per dimension.  Grant
----- Original Message -----
From: "Jerry Frost" <frosty at customcpu.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Saturday, April 16, 2005 12:37 PM
Subject: Re: [TheForge] Steel weight


> 0.28 lbs./cu/in. is plenty accurate, easy to remember and calculate.
>
> Frosty
> ------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
>
> Meadow Lakes, AK.
>
>
> From: "Phlip" <phlip at 99main.com>
>
> Subject: [TheForge] Steel weight
>
>
>>
>> Anybody know where, on line, I might be able to find a table of 
steel
>> weight
>> per running foot? I need to buy some stock, and since they price it 
by
>> the
>> weight, and I figure out how much I need by the foot, I thought it 
might
>> be
>> helpful if I knew what the conversion is.
>>
>> Saint Phlip,
>> CoD
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________



_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list