>Thanks Justin & Charles,  I'd painted my 25# LG with Hammerite about 12
>years ago and it's done great, grease and oil and cold and hot, so Iknow
>it's not rocket science... just can't find hammerite anymore.  And, though
>it worked well for the hammer, I've had mixed results in the past with it.
>Perhaps my prep.


The local hardware store here still has hammerite. However Rustoleum has a
simmilar hammered finish paint now that comes in great collors, goes on over
rust, requires no primmer and lasts as well as the hammerite in my
experience. It is cheaper too.