When my customer requests meteorite in a knife, I forge it into a damascus
pattern with medium carbon steel, and make the hilt and pommel with it.
It's best not to use it in the blade except maybe in mosaic damascus, as a
small portion of the pattern, in a non critical area of the blade.
Chuck
----- Original Message -----
From: "Phlip" <phlip at 99main.com>
To: <theforge at mailman.qth.net>
Sent: Wednesday, June 09, 2004 3:19 PM
Subject: [TheForge] Meteoric iron
>
> Looks like I'm going to have some high nickle iron from a meteor to play
> with- any suggestions for working it?
>
>
>
>
>
> Saint Phlip,
> CoDoLDS
>
> "When in doubt, heat it up and hit it with a hammer."
> Blacksmith's credo.
>
> If it walks like a duck, and quacks like a duck, it is probably not a
> cat.
>
> Never a horse that cain't be rode,
> And never a rider who cain't be throwed....
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list