Phlip go to my site
http://home.earthlink.net/~chevalvolant/flyinghorseforge.html and look under
knife you will see the knife I forged from a meteorite.
this stuff is strange I found you had 3 hits when you were at temp. this was
from the 1962 Russia site the stuff I got from china sucked.if it is high
enough Iron/nickel you can forge it. if not not
Dan
>
> Looks like I'm going to have some high nickle iron from a meteor to play
> with- any suggestions for working it?
>
>
>
>
>
> Saint Phlip,
> CoDoLDS
>
> "When in doubt, heat it up and hit it with a hammer."
> Blacksmith's credo.
>
> If it walks like a duck, and quacks like a duck, it is probably not a
> cat.
>
> Never a horse that cain't be rode,
> And never a rider who cain't be throwed....
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list