I feel they will have a dirt problem if they are on
the end of the post.
I made a split bronze barring thing that fit around
the  gate back,   but I had to turn a round section
one foot up and one foot down on the square post..

I use the word Post meaning the back vertical part of
the gate...


If it was me, I would just order up some barrel hinges
and weld them on and grease them up and forget about
them for a long long while...

Mike Wolfe








--- Dan Scheid <damales at earthlink.net> wrote:
> ok I'm working on a design for a swing gate 5' tall
> 6' wide made of 1" and
> 1/2" steel. For the hinge I was thinking of using a
> post with barring. So
> the hinge is not visible. The question is what type
> of barring would you
> recommend? We are dusty and dirty out here in sunny
> Ca. so I'm worried about
> the hinge filling in with grit . Any and all input
> is welcome
> Dan Scheid
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 


More information about the TheForge mailing list