I've only done very basic stuff, mainly the bowls for ladles.  It makes for
a nice mixed media pice with the copper bowl and forged handle.  I did a
colaboration piece with my son for the BAM comference auction last year. He
made some damascus which I forged into a handle and then he finished.  He
did most of the work, he hand sands the finish on his damascus before
etching.