There are various cleaning/pickeling formulas based on phosphoric acid which
have been used successfully over the years by the ornamental iron industry.
The concentrate is available from suppliers like Jansen or Decorative
http://www.decorativeiron.com/?a11=CLEANERS%2C%20FINISHES&page=cleaners__finishes
A friend of mine uses a concentrated industrial detergent called Greased
Lightening with some success.