> Fonde
> There are various cleaning/pickeling formulas based
> on phosphoric acid which 
> have been used successfully over the years by the
> ornamental iron industry. 
> The concentrate is available from suppliers like
> Jansen or Decorative 
>
http://www.decorativeiron.com/?a11=CLEANERS%2C%20FINISHES&page=cleaners__finishes
> 
>  A friend of mine uses a concentrated industrial
> detergent called Greased 
> Lightening with some success.
> 
> 
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post
> was in HTML
> or had an attachment.  Attachments are not allowed. 
> To learn how
> to post in Plain-Text go to:
> http://www.expita.com/nomime.html  ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
> 


__________________________________
Do you Yahoo!?
Find out what made the Top Yahoo! Searches of 2003
http://search.yahoo.com/top2003