[TheForge] superquench questions
Bruce Freeman
FREEMAB at pt.fdah.com
Tue Dec 28 08:31:10 EST 2004
As far as I can tell, none of those three products even remotely
resembles Basic I.
A better bet might be a photographic wetting agent, as has been
suggested by some.
I don't have this as a fact, but it appears that Basic H may be Basic I
diluted 1:1 with water.
However, in the USA, Basic I is easily available through distributors.
Substitutions are not really necessary.
Bruce
NJ
>>> sos at alum.mit.edu 12/27/2004 9:20:30 PM >>>
Jet Dry, Simple Green, and Calgon are mentioned various places on the
web as substitutes for Basic I. I haven't tried it. You can read
several
opinions here:
http://www.reil1.net/theforge1.html
where you can also find the recipie. Search (control F on Windows) for
superquench.
If you are using mild steel, these days it isn't so mild. Keep an eye
on
your dies to make sure they don't crack (good idea whether you use
superquench or not).
Welding beads may have higher carbon than the surrounding steel,
possibly too high for superquench (it may crack or be too brittle.
Not that I've used much superquench in the past 8 years or so, no
expertise here.
Steve
Schade wrote:
>
> I bought a set of the dovetail die adaptors for my LG 25 from Sid. I
> have some chunks of 2"x3" to make a few sets of dies.
>
> Do any of you use "superquench" on hammer dies?
>
> What is the current recipe?
>
> Is there somewhere online to get the Shaklee stuff?
>
> Has anyone ever Rockwelled after superquenching?
>
> Should I weld the die together before superquenching?
>
> Is a 5 gallon bucket of SQ big enuf to quench hammer dies?
>
> Thanks.
>
> Bob
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list