Don't know if it will affect you, but most copper grounding rod is
actually iron with a really heavy layer of copper. Looks more like it
has been dipped than plated.
Charles
Justin Fellenz wrote:
>Aaron, have you thought about welding? I've had good luck welding
>copper together using tig and regular single strand electrical wire for
>filler, and I bet you could do it with gas too. Copper runs really
>smoothly, it just takes a lot of heat, and the whole piece gets hot
>real fast, almost like water running up a pipe. It gets all black and
>nasty looking but scotch-brite makes it nice again. The nice thing
>about welding is that you have all one color of metal--you can make it
>look like it grew that way.
>
>Just a thought.
>
>JRF
>
>